Why is calcined kaolin used for press strength?
Because the calcination step creates a harder, more angular particle that interlocks under pressure instead of sliding past its neighbours.
Soft platy fillers such as talc and mica slide, which is what gives slip but also what lets a compact crumble. Calcined kaolin particles key into each other and hold the structure. In a talc-reduced compact, that is often the reason the formula still presses at all.
The practical limit is feel: above roughly 15% the compact starts to feel dry and chalky on application.
| Market | Status | Basis and conditions |
|---|---|---|
| EU | Permitted | CosIng listed; no Annex restriction — Crystalline silica is classified Carc. 1A by inhalation, but cosmetic kaolin is a hydrated aluminium silicate, not free crystalline silica; the respirable crystalline silica content belongs in the specification. |
| UK | Permitted | No Annex restriction |
| US | Permitted | No ingredient-level restriction |
| China | Permitted | IECIC |
| Japan | Permitted | General cosmetic ingredient |
| ASEAN | Permitted | ACD, no Annex entry |
| Korea | Permitted | MFDS cosmetic ingredient standard |
| Canada | Permitted | Hotlist: not listed |
Swipe the table sideways for the full basis column →
Watch: None. Note that "crystalline silica" restrictions apply to free crystalline silica, not to kaolinite.
Checked November 2026. Summary only — every material in the same format. Not legal advice; verify before labelling.