Cosmetic Powder Knowledge Base
279 answered questions, filed under 9 sections and 25 topics. Every answer has its own page — bookmark it, forward it to a colleague, or cite it as a technical reference.
All answers279
Formulation & Process
Pressing crumble, pilling, white cast, lipstick sweating — what to adjust, by symptom.
003Which powders give a natural soft-focus effect?Soft focus means scattering light at the skin surface instead of reflecting it directly. At the powder level that requires two things: a particle size distribution close to the wavelength scale, and s…› 011How do I choose pore size for oil absorption?Pore size decides two things: how fast oil goes in and how much the particle can hold. Three bands cover most work. Small pores at 5-15 nm with 300-500 m2/g surface area exert strong capillary force, …› 013Can oil control and moisturising coexist?Yes, but through selective absorption rather than a higher absorption dose. The conflict is that powder cannot tell sebum from the emollient oil in the formula, so it takes both, and oil control ends …› 015How do I build a blended oil-absorption system?One powder is usually not enough, because absorption has to meet three conflicting demands at once: absorb fast, hold a lot, and not collapse once loaded. Divide the work three ways. Small pores with …› 016Does hydrophobic treatment improve oil control?Usually yes, but not because it absorbs more. It absorbs more selectively and keeps what it takes. There is a cost, and it should be planned for. Three benefits. First, selectivity: a hydrophobic surf…› 019Does powder affect lipstick transfer?It matters, but powder is not the main variable. Transfer is set largely by the film-forming system and the wax ratio, with powder as a secondary adjustment. Being clear about this saves effort, becau…› 028Is grittiness in lip mud caused by coarse powder?Check dispersion before blaming particle size. In practice about seven out of ten "gritty" complaints turn out to be agglomerates, and an agglomerate behaves like a particle several times larger than …› 029What does powder do for transfer-resistant wear?Powder helps in three places, and none of them is adhesion. First, it takes up excess oil. Transfer is oil from the lips moving to the cup wall, so absorbing free oil reduces what can transfer. Spheri…› 030How do I stop a clay mask from drying tight?The tightness is usually not about total oil uptake but about how steep the uptake curve is: the mask pulls oil and water out within minutes and the skin reads that as tight. Three powder-side levers.…›
Powder Materials
Boron nitride, spherical silica, mica, talc and pigments — how to choose, which system each fits.
Regulation & Compliance
EU, Japan and China requirements, export documents, and how restricted substances are verified.
Ordering & Samples
Sampling, MOQ, lead times, how quotes are built, custom surface treatment — confirm before ordering.
061What is the minimum order quantity?For standard grades the MOQ follows the packaging format, typically one 25 kg drum, with some higher-value grades available in 5 kg or 10 kg packs. Custom-treated powders carry a higher MOQ because su…› 064Can you provide COA, MSDS and TDS?Yes, all three. The COA is issued per batch with measured values for that batch; the MSDS follows the standard format; the TDS gives typical properties and application guidance. Do not confuse them. T…›
Production & QC
How D50 is measured, batch-to-batch control, preventing agglomeration, retention samples, issue handling.
071How do you control batch-to-batch variation?Three things: a stable raw material source, fixed process parameters, and per-batch testing before shipment. Powder production is most exposed to changes in deposit or supplier; once the impurity prof…› 074Do you keep retention samples and for how long?Yes. Retention samples are kept for a defined period after each batch ships, with the duration depending on product type and customer agreement. Custom grades are retained longer because they correspo…› 075How are quality issues handled?Step one is always to freeze the information: keep the physical sample from the affected batch, record the use conditions, and establish how the anomaly can be reproduced. Without those three, any con…›
After-Sales Support
Caking on arrival, batch colour drift, mismatched retest data, dispersion failures, storage spoilage — how to judge, and what to do next.
090How do we confirm that only one batch is affected?Through batch traceability. Our records cover three things: raw material lot, production batch, and retention sample plus shipment routing. Given a batch number, we can tell which customers received t…›
Wet-Stripped Boron Nitride15 answers
Spherical Porous Silica14 answers
107How do I choose between oil absorption 60 and 300?By how much oil you need taken out of the formula, and how dry you can afford the finish to feel. Low oil absorption (Kingsica S060 at 60, TR070SI at 70) suits formulas that already contain enough oil…› 109Which grade gives soft-focus, and at what loading?The fine, mid-absorption spherical grades — 2028 at 2 µm and 3028 at 3 µm — are the usual starting point, typically at 2–6%. Soft-focus comes from the spherical shape and the pore-size distribution ra…› 110Which grades are for scrub and cleansing textures?The PC series — PC20 (20 µm), PC100 (100 µm), PC150 (150 µm) and PC200 (200 µm), at oil absorption 100–130. For scrubs the particle size sets the sensation: 100–200 µm reads as a clearly perceptible s…› Titanium Dioxide13 answers
121Rutile or anatase: which one should I start with?Rutile for almost everything, anatase only where you want a specific optical effect. Rutile scatters light more efficiently and is the grade the industry builds coverage around, so it reaches the same…› 128What paperwork comes with each lot?A batch COA, the TDS, and the SDS. Additional documents — heavy metal statements, allergen declarations, non-nano statements, REACH registration status — are issued on request against the specific gra…› 130What are MOQ, lead time and packaging?MOQ is typically 25 kg for a stock grade and 100–200 kg for a production run of a non-stock grade. Lead time is roughly 7–15 working days depending on grade and quantity; stock items ship sooner. Stan…› Calcined Kaolin11 answers
1355000 at 2 µm or GL03 at 3 µm?2 µm if you want maximum oil absorption and a matte finish; 3 µm if you want easier dispersion and a less dry feel. The finer grade has more surface per gram, so it takes up more sebum and gives a fla…› 143What is the MOQ and how is it packed?25 kg per bag as standard, with 500 kg jumbo bags for volume orders. MOQ for a stock grade is 25 kg; a non-stock grade is typically 100–200 kg. Lead time runs about 7–15 working days. Samples are 1 kg…› Talc13 answers
149What is the BVL series, and do I need it?It is the same talc held to the German BVL heavy-metal limits, which are stricter than the general cosmetic specification and are used as a reference by a number of European customers. You need it if …› 151How do I keep talc from flying during filling?Reduce the fine fraction and control humidity, in that order. Airborne dust during filling is mostly the sub-10 µm fraction, and a coarse grade such as LS-325 generates noticeably less of it than a 5 …› 152Can I replace talc completely?In most formulas, yes, but it takes more than one material. Talc does three jobs at once — slip, oil absorption and cost — and no single substitute does all three at the same price. The usual approach…› 153Does particle size affect adhesion and wear?It affects them through the oil absorption path more than directly. Finer talc with higher oil absorption takes up more of the binder and the sebum, which can improve wear because the film stays drier…› 157Does talc cake up once it absorbs oil?Talc absorbs comparatively little oil and absorbs it slowly, so it is one of the less caking materials in a powder — that is part of why it was the default for so long. What caking it does show usuall…› Wet Ground Mica13 answers
163Is there a BVL grade in the mica range?Yes — Kingcovite 6710 at 10 µm, held to the German BVL heavy-metal limits. It sits in the synthetic fluorphlogopite group, which is where the strictest market requirements usually land, because the sy…› 166What is the MOQ and what packing do you use?25 kg per bag, 500 kg jumbo bags available. MOQ 25 kg for stock grades, 100–200 kg for non-stock. Lead time is about 7–15 working days; samples are 1 kg and ship with COA and TDS. Mica is a low-bulk-d…› 169Why does mica feel so good on skin?Because it is flat, and flat things lie down. The platelets are thin relative to their width, so they settle parallel to the skin instead of standing on edge, and the surface your finger meets is a sm…›
Cosmetic Pigments11 answers
177Which lakes can I use in lip products?Check the market's permitted list by CI number and by product category — that is the only reliable test, because the answer differs between the EU, the US and China for the same lake. As a starting po…› 178How do I compare light fastness between two grades?Test them in your own base under your own conditions — a light fastness rating on a datasheet is a starting filter, not a result. The published ratings in our water-soluble dye series (the star rating…› 180What are the MOQ and lead time for pigments?MOQ is 1 kg for a stock grade and 25 kg for a production quantity; some specialty lakes have a 5 kg minimum because they are made to order. Lead time is 7–15 working days, longer for a non-stock lake.…› Pigment Formulation9 answers
189Why does colour rub off a pressed powder?It is adhesion and compatibility, not a pigment that is inherently loose. Three causes. The pigment does not bond to the platelet fillers — talc, mica — so it sits at the surface and wipes away. The f…› Oil-based Slurry14 answers
198What is the MOQ and the shelf life?MOQ is 5 kg for a stock grade and 25 kg for a production quantity; a custom carrier is 100–200 kg. Shelf life is typically 24 months from production in an unopened container. Lead time is 7–15 working…› Water-based Slurry14 answers
211What are the eyeliner and nail polish series?They are the same dispersion technology tuned for two applications with unusual demands. The high-waterproof eyeliner series is built for films that stay on a wet lash line without smearing, so the di…› 212What is the MOQ and lead time?MOQ is 5 kg for a stock grade and 25 kg for production. Lead time 7–15 working days, samples 1 kg. Shelf life is typically 12 months for water-based products, shorter than the oil-based range because …› Allochroic Particles11 answers
221Why does the colour not shift in my formula?Usually because the particle is fully wetted and stays wetted, so there is no change in its local environment to trigger the shift. The effect depends on the particle experiencing a change — typically…› 222What loading do you recommend?1–5%, with the effect becoming obvious around 2–3%. Below 1% the shifted colour is too diffuse to read as a deliberate effect, and it looks like an off-shade rather than a colour change. Above 5% the …› 223How stable are they over shelf life?Stable in a properly formulated base, but they are the most process-sensitive material in our range — handle them accordingly. The shell is the functional part, so anything that damages it also kills …› 225Is the change reversible?In use, the shift is intended to be a one-way visual effect within the application — the product changes as it is applied and does not return to the original colour on the skin. That is the point of t…› 226What is the MOQ and how should it be stored?MOQ is 1 kg for a sample and 25 kg for production. Lead time 7–15 working days. Store sealed, at 15–30 °C, away from direct light and away from strong odours — the shell can pick up volatile compounds…›
Surface Treatment13 answers
230When is a surface treatment worth paying for?When the powder has to survive a system it was not born to live in — a silicone phase, a W/O emulsion, a high-humidity wear claim, or a compact that has to press hard. Untreated mineral powder is hydr…› 232Can the SI treatment be applied to any grade?Yes — to all series and particle sizes. That is stated on the page and it is the practical advantage of the range. So Kingbornit 3002 SI, Kingsica 3028 SI, Kingruti 0205 SI, Kingtalfer LS-800 SI and K…› 239Is there a treatment for a hydrophilic system?Yes — the hydrophilic treatment exists for water-based and O/W systems where you want improved dispersion without making the surface hydrophobic. It is the counterpart to the lipophilic treatments: in…› 240What is the MOQ for a treated grade?25 kg for a stock treated grade; a treatment applied to a grade we do not normally carry is 100–200 kg, because the treatment line has to be set up and cleaned. Lead time is 7–15 working days for stoc…› Surface Treatment Application 10 answers
247Which processes break down a treatment layer?Three-roll milling, bead milling, high-shear homogenising, and long hot emulsification. All four apply shear and heat together, which is what a treatment layer tolerates least. When the layer fails yo…› 250Can treatment stop a heavy powder from settling?It helps, but it cannot change the physics. Settling is a density and particle-size problem; treatment only changes surface compatibility. What treatment does: better compatibility with the continuous…› Inorganic Sunscreen13 answers
253Nano TiO2 or nano ZnO — which should I use?ZnO for UVA coverage and TiO2 for UVB and the higher refractive efficiency; many serious formulas use both. ZnO has a wider absorption band that extends further into UVA, which is why it appears in pr…› 256Powder or pre-dispersion?Pre-dispersion if you can — it solves the hardest problem in the formula, which is wetting a nano powder completely. Nano powders have enormous surface area and agglomerate readily; getting them fully…› 257How do I choose the carrier for a pre-dispersion?Match it to your emollient system and to the feel you want — the carrier becomes part of the formula. C12-15 alkyl benzoate (4015, 4513, 4560, Z-6060) is the general-purpose choice: light, dry, widely…› 258How much do I need to reach a given SPF?As a rough starting point, 5–10% combined inorganic solids gets you into the moderate-SPF range, and 15–25% is where mineral-only high-SPF formulas live — but the number that matters is measured in yo…› 259Does the coating matter for photostability?Yes — it is the main lever you have over the photocatalytic activity of the particle. TiO2 and ZnO generate reactive species at the surface when they absorb UV, and those species attack the surroundin…› 260How do I reduce the white cast?Smaller particle size, better dispersion, and if necessary a lower loading with an organic filter carrying the rest of the SPF. White cast has two causes. Undispersed agglomerates scatter visible ligh…› 261What testing documents do you provide?We provide the material documentation: COA, TDS, SDS, and the nano-specific statements a market may require. The finished-product testing — SPF, UVA-PF, critical wavelength, water resistance — is done…› 264Can a mineral sunscreen be made as a spray?Yes, but only as a pump spray, and the formulation window is narrow. A pressurised aerosol with mineral filters is a problem on two counts: the powder settles in the propellant system, and the inhalab…› Sunscreen Formulation8 answers
Others6 answers
275What does the sample programme include?1 kg of powder or 5 kg of a dispersion, with COA, TDS and SDS. Samples are free; you cover the freight. For a first evaluation, ask for two grades rather than one — the comparison is what tells you wh…› 276What documents come with a shipment?COA per lot, TDS per grade, and SDS. Beyond that, the regulatory statements a market requires — heavy metal declarations, non-nano or nano statements, allergen declarations, REACH status, BSE/TSE stat…› 277What are the general order terms?MOQ 25 kg for a stock grade, 100–200 kg for a custom grade or a custom carrier. Lead time 7–15 working days for stock, longer for custom. Payment terms are confirmed at quotation and depend on the mar…› 279Which grades are outside these twelve categories?This page is the catch-all for materials that do not sit cleanly in one of the other product families — specialty fillers, materials in development, and combinations that are made to order. If you can…›
No answer matches your search. Try pilling, D50, talc or MOQ.
Not finding an answer?Describe your formulation system and the problem — the technical team replies within one business day, and can arrange samples at the same time.
Talk to our technical team