You are using an outdated browser. For a faster, safer browsing experience, upgrade for free today.
Spherical Porous Silica

How do I stop silica from agglomerating in the premix?

Wet it out before it goes into the main batch, and keep the shear high enough while it disperses.

Spherical porous silica has a large internal pore volume, so it pulls binder and oil into the pores quickly and forms lumps that are hard to break down later. Adding it into a portion of the oil phase first, or under higher shear than the rest of the batch, usually resolves it. Adding it last into a low-shear batch is the most common cause.

If agglomeration appears only after storage rather than during making, the cause is usually insufficient wetting rather than the grade, and changing grade will not fix it.

Regulatory status — Silica (synthetic amorphous) INCI SILICA · CAS 7631-86-9, 112945-52-5
MarketStatusBasis and conditions
EU Permitted CosIng listed; no Annex restriction — Synthetic amorphous silica is not the same substance as crystalline silica, which carries a Carc. 1A inhalation classification. Nano forms must be labelled "[nano]" under Article 19(1)(g).
UK Permitted No Annex restriction
US Permitted No ingredient-level restriction
China Permitted IECIC
Japan Permitted General cosmetic ingredient
ASEAN Permitted ACD, no Annex entry
Korea Permitted MFDS cosmetic ingredient standard
Canada Permitted Hotlist: not listed

Swipe the table sideways for the full basis column →

Watch: None. Keep the distinction between synthetic amorphous silica and crystalline silica explicit — most compliance questions on this material come from that mix-up.

Checked November 2026. Summary only — every material in the same format. Not legal advice; verify before labelling.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.
Become a Distributor