Can powder selection fix chipping edges and poor pickup?
Partly. Chipping in a multi-pan palette behaves differently from a single pan: most of it sits at the boundaries between pans and at the rim. That is an edge effect — the press head transfers pressure unevenly at the edge and demoulding adds shear, so the edge fails first. Powder choice helps, but tooling and rest time matter as much.
Four levers. First, raise green strength: more platy powder (talc, mica, boron nitride) improves interlocking, and it is the most direct move. Second, add binder. Metal soaps such as magnesium stearate or zinc stearate, or a small amount of oil, raise green strength at typically 1-3%; too much soap gives a soapy feel and hurts pickup. Third, set the pressure. Too low and the cake is loose; too high and internal stress causes spring-back cracking after demoulding — find the window rather than pressing harder. Fourth, look at demoulding and tooling. Multi-pan cavities are shallow with thin walls, so uneven ejection force is the usual cause; corner radius and ejection synchronisation matter more than the formula.
Two factors specific to palettes. Each pan has its own formula: matte and pearl pans compress very differently, so one pressure setting will fail the less compressible pan. And rest after pressing: a palette moved straight to assembly has not released stress and fails in transit — leave it 12-24 hours.
Judge with a drop test plus transport simulation (vibration table or drop), because visual inspection does not reveal internal cracks.