001When is a surface treatment worth paying for?When the powder has to survive a system it was not born to live in — a silicone phase, a W/O emulsion, a high-humidity wear claim, or a compact that has to press hard. Untreated mineral powder is hydr…
002There are eleven treatment types. How do I narrow it down?By what you are trying to fix — that is what separates them. Dimethicone (SI) is the general-purpose choice: chemically bonded, shear-resistant, works over a wide temperature range, gives strong water…
003Can the SI treatment be applied to any grade?Yes — to all series and particle sizes. That is stated on the page and it is the practical advantage of the range. So Kingbornit 3002 SI, Kingsica 3028 SI, Kingruti 0205 SI, Kingtalfer LS-800 SI and K…
004Does a surface treatment change the colour or the coverage?Very little, and what does change is the dispersion, which can look like a colour change until you know why. The treatment is a molecular layer on the surface, so it does not alter the refractive inde…
005What is the difference between triethoxycaprylylsilane and dimethicone treatment?Both make the surface hydrophobic; the silane does it without adding a silicone feel, which is why it dominates in UV filters. Triethoxycaprylylsilane bonds directly to the surface hydroxyls and gives…
006How do I verify that the treatment is actually there?Three quick checks, in increasing order of effort. First, the water float test: a treated powder floats on water and an untreated one wets and sinks. It is crude but it tells you immediately whether t…
007Does treating a powder affect its regulatory status?Yes, in the sense that the treatment agent becomes part of the ingredient declaration and must itself be permitted. A treated powder is not the same regulatory object as the untreated one: the coating…
008Do I need to change the loading when I switch to a treated grade?Usually not — start at the same loading and adjust on the result. The treatment is a small weight percentage on the surface, so the delivered pigment or powder content per kilo is essentially unchange…
009What loading of treated powder do you see in a W/Si system?It depends on the powder, but the treated grades are what make high loadings possible in silicone-continuous systems. In a W/Si foundation, treated TiO2 and treated iron oxides commonly run at 8–15% c…
010Is there a treatment for a hydrophilic system?Yes — the hydrophilic treatment exists for water-based and O/W systems where you want improved dispersion without making the surface hydrophobic. It is the counterpart to the lipophilic treatments: in…
011What is the MOQ for a treated grade?25 kg for a stock treated grade; a treatment applied to a grade we do not normally carry is 100–200 kg, because the treatment line has to be set up and cleaned. Lead time is 7–15 working days for stoc…
012What dosage of treatment agent is used, and what happens if it is too low?Treatments are applied at roughly 1–3% on the weight of the powder, depending on the agent and the surface area of the grade. A finer powder needs more, because there is more surface to cover. Too low…
013I changed treatment supplier on the same base powder. What has to be re-qualified?Treat it as a new raw material, not as a purchasing change. The base powder is the same; the surface chemistry is not, and the surface is what your formula interacts with. Re-qualify in this order. Di…
Surface Treatment Application 10 answers
014Treatment dosage scales with surface area. How do I set it for a new grade?There is no universal figure. Dosage is set per powder, from its specific surface area and from what you want the treatment to do. The rule is straightforward: the higher the specific surface area, th…
015How far does oil absorption drop after treatment — and when is that a problem?Usually a clear drop, and the size of it depends on agent type and coverage. For most formulas that drop is the main reason to pay for treatment. The mechanism: the agent occupies active sites on the …
016Does treatment change SPF enough that I have to re-test?Yes, and the direction depends on the agent and the loading. It cannot be assumed either way — it has to be measured. Two mechanisms act at once. Better dispersion means the particles sit more evenly …
017Will a treatment shift the shade enough to need re-matching?Slightly, and mostly through gloss, transparency and saturation rather than hue. Pale and bright shades are the sensitive ones. The layer changes refractive index and scattering at the surface, so wha…
018Which processes break down a treatment layer?Three-roll milling, bead milling, high-shear homogenising, and long hot emulsification. All four apply shear and heat together, which is what a treatment layer tolerates least. When the layer fails yo…
019Can I claim silicone-free when the powder is SI-treated?No — not if the treatment is a silicone. This is the most common place a "silicone-free" claim fails. "SI" is a family label, not an ingredient. The agent may be dimethicone, a polymethylsiloxane or a…
020Switching from one treatment type to another — what is the full re-test list?Six items minimum: dispersion, viscosity, stability, skin feel, colour where a pigment is involved, and whatever functional claim the product makes. Dispersion and viscosity move first, because the ag…
021Can treatment stop a heavy powder from settling?It helps, but it cannot change the physics. Settling is a density and particle-size problem; treatment only changes surface compatibility. What treatment does: better compatibility with the continuous…
022Does treatment raise tinting strength? Do I have to cut the loading?Yes, usually — and yes, expect to cut the loading when you move from an untreated to a treated pigment. The gain is a dispersion effect, not a stronger pigment. Fewer agglomerates mean more effective …
023How do I prove a treatment is working, layer by layer?Four layers, in this order: surface properties, dispersion state, formula performance, then stability. Skipping to the last one is why treatments get blamed for problems they did not cause. Surface fi…
Inorganic Sunscreen13 answers
024Nano TiO2 or nano ZnO — which should I use?ZnO for UVA coverage and TiO2 for UVB and the higher refractive efficiency; many serious formulas use both. ZnO has a wider absorption band that extends further into UVA, which is why it appears in pr…
025Nano or non-nano? What is the regulatory difference?It is the single most consequential decision in an inorganic sunscreen, because nano status changes the notification route, the labelling and the safety dossier. Most markets define nano by primary pa…
026Your grades run from 15 nm to 160 nm. What does size change?Smaller particles give more transparency and better SPF per unit mass; larger ones give less whitening but require more loading, and above a certain size the UV performance starts to drop. 15 nm (N15E…
027Powder or pre-dispersion?Pre-dispersion if you can — it solves the hardest problem in the formula, which is wetting a nano powder completely. Nano powders have enormous surface area and agglomerate readily; getting them fully…
028How do I choose the carrier for a pre-dispersion?Match it to your emollient system and to the feel you want — the carrier becomes part of the formula. C12-15 alkyl benzoate (4015, 4513, 4560, Z-6060) is the general-purpose choice: light, dry, widely…
029How much do I need to reach a given SPF?As a rough starting point, 5–10% combined inorganic solids gets you into the moderate-SPF range, and 15–25% is where mineral-only high-SPF formulas live — but the number that matters is measured in yo…
030Does the coating matter for photostability?Yes — it is the main lever you have over the photocatalytic activity of the particle. TiO2 and ZnO generate reactive species at the surface when they absorb UV, and those species attack the surroundin…
031How do I reduce the white cast?Smaller particle size, better dispersion, and if necessary a lower loading with an organic filter carrying the rest of the SPF. White cast has two causes. Undispersed agglomerates scatter visible ligh…
032What testing documents do you provide?We provide the material documentation: COA, TDS, SDS, and the nano-specific statements a market may require. The finished-product testing — SPF, UVA-PF, critical wavelength, water resistance — is done…
033What are the MOQ and lead time for sunscreen grades?MOQ is 1 kg for a powder sample and 5 kg for a pre-dispersion sample; production quantities start at 25 kg. Lead time is 7–15 working days for stock grades, longer for a custom carrier. Because nano m…
034Why does my mineral sunscreen pill or roll up?Pilling is a film problem, not a pigment problem, and it usually has one of three causes. The first is an incompatibility between the sunscreen film and the product applied underneath. A mineral sunsc…
035Can a mineral sunscreen be made as a spray?Yes, but only as a pump spray, and the formulation window is narrow. A pressurised aerosol with mineral filters is a problem on two counts: the powder settles in the propellant system, and the inhalab…
036Can bismuth oxychloride be used as a UV filter?No. In cosmetic formulas bismuth oxychloride (CI 77163, Kingbismo® range) works as a pearlescent and soft-focus colorant: its plate-like crystals reflect visible light to give a satin lustre, but they…
Sunscreen Formulation8 answers
037White cast and grey cast are not the same problem — how do I tell them apart?White cast is scattering; grey cast is usually hue. They take different fixes, so diagnose before reformulating. White cast comes from visible-light scattering by particles whose size is comparable to…
038Pilling gets worse when I layer foundation over sunscreen — whose problem is it?Usually the interface, not either product on its own. A mineral sunscreen built on a W/O emulsion leaves a film that a water-based foundation then sits on. The two films shear against each other as th…
039SPF does not scale with filter loading — where is the knee?It rises, then flattens, and past the knee it can fall. Do not size the loading from a linear calculation. More filter means more shielding per unit area, so SPF climbs. Then the marginal return drops…
040The carrier counts as oil in my formula — how much do I subtract?All of it, by mass. A pre-dispersion is a raw material that brings oil with it, and that oil is in the formula whether or not it was counted. Our dispersions come in several carriers: C12-15 alkyl ben…
041How do I test whether a mineral sunscreen will oxidise in the bottle?Accelerated light exposure plus peroxide value. The coating specification tells you the risk; the test tells you the outcome. The mechanism: nano TiO2 and ZnO generate electron-hole pairs under UV, wh…
042A mineral sunscreen feels heavy and suffocating — where do I start?Powder form, oil structure, film former — in that order. Cutting the filter load is the last resort, because it costs protection. Powder first. A pre-dispersion spreads more evenly than powder dispers…
043Do pre-dispersions settle, and how do I keep batches consistent?They settle, because the particles are denser than the carrier. That is physics; the job is to keep it redispersible and to dose by solids. How fast depends on three things: particle size, since agglo…
044What does a nano spray sunscreen need before it can be notified?The inhalation route is the whole question, and it has to be settled before the formula is developed, not before launch. A spray creates an inhalable aerosol. Nano TiO2 or ZnO reaching the lung is a d…
Others6 answers
045Can you make a custom grade — a size or treatment you do not list?Yes, within the limits of the production line. Particle size classification and surface treatment are both adjustable, and a custom combination is a normal request rather than an exception. What is re…
046What does the sample programme include?1 kg of powder or 5 kg of a dispersion, with COA, TDS and SDS. Samples are free; you cover the freight. For a first evaluation, ask for two grades rather than one — the comparison is what tells you wh…
047What documents come with a shipment?COA per lot, TDS per grade, and SDS. Beyond that, the regulatory statements a market requires — heavy metal declarations, non-nano or nano statements, allergen declarations, REACH status, BSE/TSE stat…
048What are the general order terms?MOQ 25 kg for a stock grade, 100–200 kg for a custom grade or a custom carrier. Lead time 7–15 working days for stock, longer for custom. Payment terms are confirmed at quotation and depend on the mar…
049Can you help with the formulation, not just the material?Yes, within limits — we can tell you what has worked in comparable systems and what the common failure modes are, and we can review a formula for obvious incompatibilities. What we cannot do is take r…
050Which grades are outside these twelve categories?This page is the catch-all for materials that do not sit cleanly in one of the other product families — specialty fillers, materials in development, and combinations that are made to order. If you can…
No answer matches your search in this topic.
Not finding an answer?
Talk to our technical teamDescribe your formulation system and the problem — the technical team replies within one business day, and can arrange samples at the same time.