You are using an outdated browser. For a faster, safer browsing experience, upgrade for free today.
Surface Treatment

What loading of treated powder do you see in a W/Si system?

It depends on the powder, but the treated grades are what make high loadings possible in silicone-continuous systems.

In a W/Si foundation, treated TiO2 and treated iron oxides commonly run at 8–15% combined with the silicone phase, and treated fillers at 5–15%. Untreated powders at those levels would raise the viscosity past the point where the emulsion can be processed.

That is the whole commercial case for treatment in this system: it is not an improvement in feel, it is what makes the formulation possible at all.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.