Wet-Stripped Boron Nitride

What loading do you recommend in pressed powder and in loose powder?

A common starting point is 3–8%, adjusted upward for skin feel. Loadings above 15% are rare.

At low loading boron nitride mainly improves spreading and slip, and contributes little to compact strength. From roughly 5% the difference in hand feel becomes noticeable. Loose powders can go to 8–10%. Beyond that you are buying smaller and smaller improvements at a rising cost, and a high proportion of platy powder makes the pressed compact more brittle, so it chips more in transit.

If you are reformulating away from talc, the loading usually lands higher — see the replacement question below.

Regulatory status — Boron nitride INCI BORON NITRIDE · CAS 10043-11-5
MarketStatusBasis and conditions
EU Permitted CosIng listed; no Annex restriction — No concentration limit for cosmetic use.
UK Permitted No Annex restriction
US Permitted No ingredient-level restriction
China Permitted IECIC
Japan Permitted General cosmetic ingredient
ASEAN Permitted ACD, no Annex entry
Korea Permitted MFDS cosmetic ingredient standard
Canada Permitted Hotlist: not listed

Swipe the table sideways for the full basis column →

Watch: None at ingredient level. The hexagonal (h-BN) and cubic (c-BN) forms are different materials; specification sheets should state which one is supplied.

Checked November 2026. Summary only — every material in the same format. Not legal advice; verify before labelling.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.