How do I stop lipstick from sweating in summer?

Sweating is the bullet structure collapsing at elevated temperature, caused by insufficient binding between the oil phase and the powders. The most direct fix is replacing part of the talc or mica with 5-10% hexagonal boron nitride, which clearly improves heat resistance and structural rigidity.

Boron nitride works in two ways: the platelets increase mechanical interlocking between particles, forming a more stable network, and its lipophilic surface holds the oil phase on the particle surface so less free oil migrates out on heating.

If sweating persists, adjust the wax-to-oil ratio: raise high-melting waxes such as carnauba or ozokerite, or add a small amount of fumed silica for thixotropic control. Be careful, since excess wax drags on application and dulls gloss. Run a 7-day test at 45 C before locking the formula.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.
Become a Distributor