How do I keep coverage when reducing powder loading?
Heaviness is rarely about total powder loading; it is about insufficient hiding power per unit weight, which forces you to over-dose. Switching to more efficient powders lets you cut total loading while holding coverage.
Options that work: replace standard TiO2 with a finer, tighter-distribution grade, which can cut the required dose by 20-30% at equal coverage; replace some spherical powder with platy grades such as boron nitride or mica, since overlapping platelets cover more efficiently while reflecting light more softly; and introduce porous powders that soften appearance structurally rather than by opacity.
One counter-intuitive point: when powder loading drops, the oil phase usually needs to drop with it. Otherwise you get a floating, oily film that reads as heavier than before.