After-Sales Support

The powder arrived caked. Can this batch still be used?

Separate soft caking from hard caking first. If the lumps break under light hand pressure and leave no hard residue on a 40-mesh sieve, it is soft caking — usually caused by transport vibration plus surface moisture pickup. It normally does not affect performance, but measure moisture and dispersibility before feeding it into production.

If the lumps need knocking to break and the interior is dense, it is hard caking. Either the powder absorbed moisture and set, or stacking pressure bound the particles together. Feeding it directly will cause poor dispersion and film specks, and crushing it in-house is not recommended.

Document and sample at the same time: photograph the outer carton, the breach, the batch label and a cut section of the cake; retain 500 g and send us the batch number. We pull the retention sample from the same batch for parallel comparison and issue a written conclusion, which shows whether this is a transport issue or a batch issue.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.