Our retest gives different D50, whiteness and oil absorption values from your COA. Which one stands?

Compare test conditions before comparing numbers.

D50 depends on dispersion medium, dispersant type and dose, ultrasonic power and duration — a 10–20% spread between condition sets is common. Whiteness depends on instrument calibration, the standard plate and how tightly the sample is pressed. Oil absorption depends on how the endpoint is judged.

Align three things: the same method standard, the same dispersion conditions, the same endpoint. If a gap remains after alignment, retest through the arbitration route agreed in the contract — each side retains a sample and both go to the same third party, or samples are consolidated at one site and run on one instrument.

We keep retention samples for 24 months, so the same batch can be pulled and retested in parallel to establish whether the difference is in the batch or in the test conditions.

Not the answer you need? Request a sample or talk to our technical team — tell us your formulation system and dosage, and we will recommend the right grade.