Wet-Stripped Boron Nitride

Do I need the SI-treated boron nitride, and what does the treatment actually solve?

The untreated powder is already hydrophobic enough for most anhydrous systems, so the treatment is not about wetting. It is about dispersion stability and film behaviour.

The SI grade carries a surface treatment that improves compatibility with the oil phase. In practice that shows up as lower viscosity at the same loading, less settling in a fluid foundation, and a reduced binder demand in a pressed powder — you reach the same hardness with less binder.

Use it when you are running boron nitride at a high loading in a fluid system, or when the finished film needs water resistance. In a simple loose powder the untreated grade is fine and cheaper. Ask for both versions of the same particle size and compare viscosity in your own base — that is the only test that settles it.

Regulatory status — Boron nitride INCI BORON NITRIDE · CAS 10043-11-5
MarketStatusBasis and conditions
EU Permitted CosIng listed; no Annex restriction — No concentration limit for cosmetic use.
UK Permitted No Annex restriction
US Permitted No ingredient-level restriction
China Permitted IECIC
Japan Permitted General cosmetic ingredient
ASEAN Permitted ACD, no Annex entry
Korea Permitted MFDS cosmetic ingredient standard
Canada Permitted Hotlist: not listed

Swipe the table sideways for the full basis column →

Watch: None at ingredient level. The hexagonal (h-BN) and cubic (c-BN) forms are different materials; specification sheets should state which one is supplied.

Checked November 2026. Summary only — every material in the same format. Not legal advice; verify before labelling.