The boron nitride feels gritty in my formula. What is going wrong?
Almost always dispersion, not the grade. The platelets stack face to face and form soft agglomerates that a low-shear mixer will not break, so you feel clusters rather than individual platelets.
Two fixes. Pre-disperse the powder in a small portion of the oil phase at high shear before adding it to the main batch. And add it early enough that the batch is above the melting point of any wax in the formula — dropping boron nitride into a cooling batch is the usual cause of grit.
If it persists after that, check whether you are using a coarse grade. A 20 µm material reads as faintly sandy in a thin gel, and that is the powder behaving correctly rather than a defect. For a thin fluid, a 6 or 12 µm grade is the right choice.
| Market | Status | Basis and conditions |
|---|---|---|
| EU | Permitted | CosIng listed; no Annex restriction — No concentration limit for cosmetic use. |
| UK | Permitted | No Annex restriction |
| US | Permitted | No ingredient-level restriction |
| China | Permitted | IECIC |
| Japan | Permitted | General cosmetic ingredient |
| ASEAN | Permitted | ACD, no Annex entry |
| Korea | Permitted | MFDS cosmetic ingredient standard |
| Canada | Permitted | Hotlist: not listed |
Swipe the table sideways for the full basis column →
Watch: None at ingredient level. The hexagonal (h-BN) and cubic (c-BN) forms are different materials; specification sheets should state which one is supplied.
Checked November 2026. Summary only — every material in the same format. Not legal advice; verify before labelling.