You are using an outdated browser. For a faster, safer browsing experience, upgrade for free today.

Titanium Dioxide

Anatase

Anatase grade titanium dioxide, 2 grades, mean particle size 200–220 nm, whiteness 90–92. Anatase is softer than rutile with slightly lower opacity and higher whiteness, suiting foundations, sunscreens and colour cosmetics where powder hardness and brightness matter.

Product NameProduct CodeMean Particle SizeWhitenessSurface Coating Agent  
Kingruti T-01106416200 nm≥92——
Kingruti T-04106421220 nm≥90——

Cosmetic-grade titanium dioxide with high coverage, easy dispersion and light stability for sunscreen, foundation and color cosmetics.

Need a sample or technical data for Anatase?

Request sample

Titanium Dioxide — frequently asked questions

The 14 questions formulators and buyers ask most — open a card for the full answer and our reasoning.See all “Titanium Dioxide” answers (14) →

Recommended 01 / 14

Rutile or anatase: which one should I start with?

Rutile for almost everything, anatase only where you want a specific optical effect.

Read the full answer
Recommended 02 / 14

My coverage dropped after switching to a finer grade. Why?

Because fines that are not fully dispersed act as light scatterers in the wrong size range — they du…

Read the full answer
Recommended 03 / 14

My TiO2 leaves a chalky white cast. How do I fix it?

White cast is TiO2 doing its job too well in the wrong place.

Read the full answer
04 / 14

My TiO2 is not hiding well. What are the causes, and how do I fix it?

Work through three causes before you add more TiO2.

Read the full answer
05 / 14

Your rutile grades run from 210 to 420 nm. How does size change the result?

Smaller particles give more covering power per kilo but scatter less light back at you;

Read the full answer
06 / 14

What is the difference between aluminium hydroxide coating and aluminium hydroxide plus silica?

Alumina alone gives photostability and dispersion;

Read the full answer
07 / 14

What loading do you see in foundation, pressed powder and sunscreen?

Foundation usually lands at 5–12%, pressed powder at 3–8%, and sunscreen at whatever the SPF target …

Read the full answer
08 / 14

Is your TiO2 nano or non-nano? How do I document that?

It is non-nano.

Read the full answer
09 / 14

Does TiO2 whiten as much in a water-based system as in an anhydrous one?

Less, and the gap is bigger than most people expect.

Read the full answer
10 / 14

What paperwork comes with each lot?

A batch COA, the TDS, and the SDS.

Read the full answer
11 / 14

Which grade should I use in a compact where hardness matters?

T-48 or T-02 in rutile, or T-01 in anatase.

Read the full answer
12 / 14

What are MOQ, lead time and packaging?

MOQ is typically 25 kg for a stock grade and 100–200 kg for a production run of a non-stock grade.

Read the full answer
13 / 14

Does TiO2 cause photocatalytic degradation, and how do I control it?

Uncoated TiO2 is photocatalytic.

Read the full answer
14 / 14

Is TiO2 permitted in lipstick, and does it change the feel?

Yes, and it is common — it is what gives a lipstick opacity and makes a red read as red rather than as a stain.

Read the full answer

Not the question you had? Talk to our technical team, or browse the knowledge base.

Related questions

These come from other powder families that often appear alongside this product in the same formula.

  • How do I balance whiteness and coverage, and what happens if I overload titanium dioxide?

    Whiteness and coverage follow different curves: coverage depends on refractive index contrast, whiteness on reflectance. Titanium dioxide maxes out both at once, so the problem is rarely not white enough — it is too white.

    TiO2 has a refractive index around 2.6, the highest of any common cosmetic powder, and 3-5% already delivers ample coverage. Above 8% you hit three problems: the finish turns chalky and loses translucency, which is very visible in pressed and loose powders; spreadability drops and application feels draggy; and cost climbs while coverage has already plateaued.

    A layered approach works best: TiO2 for coverage at 3-5%, calcined kaolin or talc for bulking and cost, mica or boron nitride for translucency and luminosity, plus iron oxides for hue adjustment. If you want white with depth rather than white like flour, either move part of the TiO2 to a surface-treated grade or use a coarser rutile grade at D50 200-300 nm — similar coverage efficiency, noticeably better translucency.

  • How do I reduce white cast and pilling in mineral sunscreen?

    White cast comes first from refractive index contrast and particle size, and only second from the formula. Nano TiO2 and ZnO in the 30-50 nm range scatter far less visible light; above roughly 100 nm, white cast is unavoidable.

    Three practical routes: use surface-treated nano grades, since agglomerates rather than primary particles cause most of the whitening; switch to a pre-dispersed slurry to bypass the dispersion step and get a tighter size distribution; and add a small amount of spherical silica to improve spreading so the film stays thin and even.

    Pilling usually appears alongside white cast because both point to poor dispersion. If pilling persists after switching powders, check for high levels of carbomer or xanthan gum, which ball up easily during rub-in at high solids loading.

Become a Distributor