Long-wearing foundation pigment slurry, 4 grades, pigment content 50–60%. Formulated for long wear and transfer resistance; pre-dispersed in the oil phase so it can be charged directly into long-wearing foundation formulas.
| Product Name | Product Code | Pigment Content | CI No. |
| Titanium Dioxide Cosllary 869w AMQ | 131041 | 60% | CI 77891 |
| Red Iron Oxide Cosllary 116R AMQ | 131039 | 55% | CI 77491 |
| Yellow Iron Oxide Cosllary 340Y AMQ | 131038 | 50% | CI 77492 |
| Black Iron Oxide Cosllary 920B AMQ | 131040 | 50% | CI 77499 |
Oil-based pigment slurry with high pigment loading and uniform dispersion for lipstick, lip tint, concealer and oil-based color cosmetics.
Need a sample or technical data for Long-wearing Foundation Specialized Pigment Slurry?
The 14 questions formulators and buyers ask most — open a card for the full answer and our reasoning.See all “Oil-based Slurry” answers (14) →
It is a set of four dispersions built for transfer-resistant foundations, where the film has to stay…
Read the full answerSlurry if you are under roughly 200 kg per batch or you do not have a bead mill;
Read the full answerYes, and it is a sensible route, because a lipstick is an anhydrous system and the standard carriers…
Read the full answerChoose by the pigment, not by a preference for higher concentration.
Read the full answerIt makes the pigment surface lipophilic so the dispersion stays stable in the oil phase and the film wears longer.
Read the full answerYes, for a production quantity.
Read the full answerAs the pigment plus the carrier plus the treatment, which means the CI number alone is not the whole declaration.
Read the full answerSettling is normal for a high-loading dispersion;
Read the full answerMOQ is 5 kg for a stock grade and 25 kg for a production quantity;
Read the full answerThree things, and the first one catches most people.
Read the full answerDivide the pigment percentage you want by the slurry's pigment content.
Read the full answerBoth are surface treatments that make the pigment lipophilic, and both improve dispersion and wear.
Read the full answerNot normally, and it is worth understanding why rather than testing it.
Read the full answerCheck in this order: the container, the batch record, then the formula.
Read the full answerNot the question you had? Talk to our technical team, or browse the knowledge base.
Related questions
These come from other powder families that often appear alongside this product in the same formula.
Sweating is the bullet structure collapsing at elevated temperature, caused by insufficient binding between the oil phase and the powders. The most direct fix is replacing part of the talc or mica with 5-10% hexagonal boron nitride, which clearly improves heat resistance and structural rigidity.
Boron nitride works in two ways: the platelets increase mechanical interlocking between particles, forming a more stable network, and its lipophilic surface holds the oil phase on the particle surface so less free oil migrates out on heating.
If sweating persists, adjust the wax-to-oil ratio: raise high-melting waxes such as carnauba or ozokerite, or add a small amount of fumed silica for thixotropic control. Be careful, since excess wax drags on application and dulls gloss. Run a 7-day test at 45 C before locking the formula.
Heaviness is rarely about total powder loading; it is about insufficient hiding power per unit weight, which forces you to over-dose. Switching to more efficient powders lets you cut total loading while holding coverage.
Options that work: replace standard TiO2 with a finer, tighter-distribution grade, which can cut the required dose by 20-30% at equal coverage; replace some spherical powder with platy grades such as boron nitride or mica, since overlapping platelets cover more efficiently while reflecting light more softly; and introduce porous powders that soften appearance structurally rather than by opacity.
One point to watch: when powder loading drops, the oil phase usually needs to drop with it. Otherwise you end up with too little powder and too much oil, which brings stability problems related to oil exudation.
We reply within one business day with shipping arrangements and technical documents. Samples are free of charge; freight is collect or credited against your next order.